Update Time:2025-07-03 10:26:14
Under acidic catalyst and heating conditions, intramolecular dehydration occurs, eliminating one molecule of water to form styrene.
Item | Specification |
Shape | White Cylindrical |
Length | 3-8mm |
Bulk Density | 0.45±0.05g/ml |
Crushing Strength | ≥45N/cm |
Selectivity | 99% |
Conversion Rate | 99.2% |
|